Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Pro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and apparel packagingInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D1505
Thickness 25.0 microns
0.984 mil
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 28.0 MPa
4060 psi
ASTM D882
Film Tensile Strength at Yield, TD 20.0 MPa
2900 psi
ASTM D882
Film Elongation at Break, MD 850 %
850 %
ASTM D882
Film Elongation at Break, TD 770 %
770 %
ASTM D882
Flexural Modulus 1.67 GPa
242 ksi
ASTM D790
Secant Modulus, MD 0.690 GPa
100 ksi
ASTM D882
Secant Modulus, TD 0.540 GPa
78.3 ksi
ASTM D882
Izod Impact, Notched 0.245 J/cm
0.459 ft-lb/in
ASTM D256
Film Tensile Strength at Break, MD 27.0 MPa
3920 psi
ASTM D882
Film Tensile Strength at Break, TD 26.0 MPa
3770 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Brittleness Temperature <= -10.0 °C
<= 14.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 55 %
55 %
ASTM D2457