Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.690 GPa | 100 ksi | ASTM D882 |
DuPont™ Dartek® B-601 Nylon 6,6 Barrier Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A strong transparent nylon type 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. Can be pri.. |
|||
Secant Modulus, MD | 0.690 GPa | 100 ksi | ASTM D882 |
DuPont™ Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A cast nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylen diamine. It contains all the excellent properties .. |
|||
Secant Modulus, MD | 0.690 GPa | 100 ksi | ASTM D882 |
DuPont™ Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is special.. |
|||
Secant Modulus, MD | 0.690 GPa | 100 ksi | ASTM D882 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Secant Modulus, MD | 0.690 GPa | 100 ksi | ASTM D882 |
SCG Chemicals EL-Proâ„¢ P602F Polypropylene Film Resin Key Characteristics:Excellent optical propertiesHigh productivityRecommended Applications:Water quenched blown film for food and apparel packagingCan be blended with P600 for excellent clarityInform.. |