Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792 |
S&E Specialty Polymers GPP1005HF Series PP Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792 |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 1183 |
Solvay Engineered Polymers DEXFLEX® E756 TPO
(discontinued **) Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug.. |
|||
Specific Gravity | 0.910 - 0.913 g/cc | 0.910 - 0.913 g/cc | ASTM D1505 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 2781 |
Kraton® G1650 E (SEBS) Linear Block Copolymer Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 2781 |
Kraton® G1651 E (SEBS) Linear Block Copolymer Description: Kraton G1651 E is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 31.5% mass. It is supplied from Europe in the physical forms .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 2781 |
Kraton® G1652 E (SEBS) Linear Triblock Copolymer Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2264B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2320 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 131E Adhesive, Extrusion Grade DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, s.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 15°C; ASTM D1298 |
ExxonMobil Gargoyle Arctic 155 Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green P30336 Concentrate Based In Homopolymer PP DescriptionPOLYBATCH® P30336 is a green color concentrate based in Homopolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 15°C; ASTM D1298 |
ExxonMobil Gargoyle Arctic 300 Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity a.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D4025 |
Kraton® G1702 H (SEP) DiBlock Copolymer Description: Kraton G1702 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 28%. It is supplied from North America in the physical form ide.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Lucent Polymers PPC-310 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
PolyOne Synprene® IT 62-001 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeNaturalTransparentUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |