Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.245 J/cm | 0.459 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP600R Injection Grade Polypropylene Moplen HP600R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600R is a homopolymer typically used in injection molding of food.. |
|||
Izod Impact, Notched | 0.245 J/cm | 0.459 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene Moplen HP640R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640R is a homopolymer particularly suitable for injection molding.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7411 Polypropylene, Homopolymer Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7500 Polypropylene, Homopolymer Features: Seetec H7500 is designed for the extrusion of continuous filament (CF). This grade is characterized by medium MWD and good processability from specific additives. SEETEC H7500 meets the FD.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7511 Polypropylene, Homopolymer Features: Seetec H7511 is designed for the extrusion of staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and UV stability. SEETEC H7511 mee.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7525 Polypropylene, Homopolymer Features: Seetec H7525 is designed for the extrusion of staple fibers. This grade is characterized by Medium MWD and good thermobonding, with anti-gas fading stabilization. SEETEC H7525 meets the FD.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7600 Polypropylene, Homopolymer Features: Seetec H7600 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by medium MWD and good heat stability. SEETEC H7600 meets the FDA requ.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7630 Polypropylene, Homopolymer Features: Seetec H7630 is designed for the extrusion of continuous filament (CF) & bulk continuous filament (BCF) fibers and staple fibers. This grade is characterized by medium MWD, with anti-gas f.. |
|||
Izod Impact, Notched | 0.245 J/cm @Temperature 23.0 °C |
0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H7700 Polypropylene, Homopolymer Features: Seetec H7700 is designed for the extrusion of fine fibers with the spunbond technology. This grade is characterized by very narrow molecular weight distribution (MWD), with anti-gas fading.. |
|||
Izod Impact, Notched | >= 0.245 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.459 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3400 PP+MF40% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.245 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.459 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3400S PP+MF40% Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.245 J/cm @Thickness 3.17 mm |
0.459 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | >= 0.245 J/cm @Temperature 23.0 °C |
>= 0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Izod Impact, Notched | >= 0.245 J/cm @Temperature 23.0 °C |
>= 0.459 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, .. |
|||
Izod Impact, Notched | 0.245 J/cm | 0.459 ft-lb/in | ASTM D256 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Izod Impact, Notched | 0.245 J/cm | 0.459 ft-lb/in | ASTM D256 |
SCG Chemicals EL-Proâ„¢ P602F Polypropylene Film Resin Key Characteristics:Excellent optical propertiesHigh productivityRecommended Applications:Water quenched blown film for food and apparel packagingCan be blended with P600 for excellent clarityInform.. |
|||
Izod Impact, Notched | 0.245 J/cm | 0.459 ft-lb/in | Notched/Unnotched not specified; ASTM D256A |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Izod Impact, Notched | 0.245 J/cm @Thickness 3.17 mm |
0.459 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |