Material Notes:
LNP* VERTON* PX06419 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, Structural.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 228 MPa
33100 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 17.44 GPa
2529 ksi
50 mm/min; ASTM D638
Flexural Strength 296 MPa
42900 psi
ASTM D790
Flexural Modulus 15.23 GPa
2209 ksi
ASTM D790
Izod Impact, Notched 3.57 J/cm
6.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 16.02 J/cm
30.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D648