Material Notes:
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Water Absorption 0.19 %
<br>@Time 86400 sec
0.19 %
<br>@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 1.1 %
1.1 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 6.5 g/10 min
<br>@Load 6.60 kg,<br> Temperature 337 °C
6.5 g/10 min
<br>@Load 14.6 lb,<br> Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 114
114
ASTM D785
Tensile Strength at Break 131 MPa
19000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 6.89 GPa
999 ksi
5 mm/min; ASTM D638
Flexural Strength 227 MPa
32900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
5.12 J/cm
<br>@Thickness 3.20 mm
9.59 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 4.80 J/cm
8.99 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C
<br>@Temperature -20.0 - 150 °C
14.0 µin/in-°F
<br>@Temperature -4.00 - 302 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
<br>@Thickness 6.40 mm
410 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
<br>@Thickness 6.40 mm
410 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 220 °C
428 °F
Rate B/50; ASTM D1525
Glass Transition Temp, Tg 217 °C
423 °F
UL RTI, Electrical 170 °C
338 °F
UL 746B
UL RTI, Mechanical with Impact 170 °C
338 °F
UL 746B
UL RTI, Mechanical without Impact 170 °C
338 °F
UL 746B
Flammability, UL94 V-0
<br>@Thickness 0.400 mm
V-0
<br>@Thickness 0.0157 in
UL 94
5VA
<br>@Thickness 1.90 mm
5VA
<br>@Thickness 0.0748 in
UL 94
Oxygen Index 50 %
50 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.5
<br>@Frequency 1000 Hz
3.5
<br>@Frequency 1000 Hz
ASTM D150
Dielectric Strength 26.3 kV/mm
<br>@Thickness 1.60 mm
668 kV/in
<br>@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.0015
<br>@Frequency 1000 Hz
0.0015
<br>@Frequency 1000 Hz
ASTM D150
0.0049
<br>@Frequency 2.45e+9 Hz
0.0049
<br>@Frequency 2.45e+9 Hz
ASTM D150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI 60 - 120 sec
60 - 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
1.00 - 3.15 in/min
UL 746A
Descriptive Properties Value Comments
NBS Smoke Density, Flaming, Ds 4 min 1.3
ASTM E 662