Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | ASTM D638 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC (Asia Pacific) LNP* LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific) LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2200 PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem CRS5211 PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Tensile Modulus | 6.89 GPa @Temperature 22.8 °C |
1000 ksi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Modulus | 6.89 GPa | 1000 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |