Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 7.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Celanese Impet® 330R PET, 30% Glass Reinforced  (Unverified Data**)
Impet 330R is a 30% glass reinforced injection moldable polyester containing post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance...
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics ULTEM 2200 PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics ULTEM 2200 PEI (Asia Pacific)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics ULTEM 2200F PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D 257
SABIC Innovative Plastics Ultem 2200N PEI
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D 257
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D 257
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics ULTEM 2200R PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics ULTEM 2200R PEI (Asia Pacific)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Polyplastics FR-PET® CN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
ASTM D257
Westlake Plastics Tempalux® 20% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
1/16''; ASTM D257
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Celanese IMPET 330R PET, 30% Glass Reinforced
Impet 330R is a 30% glass reinforced injection moldable polyester containing post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance...
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Copyright © lookpolymers.com All Rights Reserved