Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end use temperature rating and good heat deformation performance as defined by UL 1581. 83 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 250 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
30S reading; ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
Type I, 50 mm/min; ASTM D638
10.0 MPa
1450 psi
50 mm/min; ISO 527
17.0 MPa
2470 psi
UL 1581
18.0 MPa
2610 psi
after 7days @113°C; UL 1581
Elongation at Break 225 %
225 %
50 mm/min; ISO 527
250 %
250 %
Type I, 5 mm/min; ASTM D638
250 %
250 %
after 7days @113°C; UL 1581
270 %
270 %
UL 1581
Flexural Modulus 0.0300 GPa
4.35 ksi
12.5 mm/min; ISO 178
0.0400 GPa
5.80 ksi
12.5 mm/min, 100 mm span; ASTM D790
Heat Distortion 20 %

@Load 0.250 kg,
Temperature 100 °C
20 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+15 ohm-cm
9.00e+15 ohm-cm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
VW-1 Pass
UL 1581
Users viewing this material also viewed the following: