Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ISO 178 |
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ISO 178 |
Polimeri Europa Greenflex® ML 50 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 50 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 50 show high elasticity.Main Applications: Greenflex.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ISO 178 |
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ASTM D790 |
ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | Tangent, 0.5 in/min; ASTM D790 |
LyondellBasell Hifaxâ„¢ CA260GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA260GC White fractional melt flow, 40 MPa flexural modulus, UV-stabilized, precolored thermoplastic elastomeric olefin (TEO) resin has an excellent balance of flexibility,.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD771 PPE-TPE (Asia Pacific) Flexible, high tensile elongation, halogen-free extrusion grade intended for evaluation in applications such as cable jacket. Flame retardant performance capable of meeting UL VW-1 requirement. 80C .. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE configurations. Flame retardant performance capable o.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Europe-Africa-Middle East) Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ASTM D790 |
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin Elvax® resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range wi.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ISO 178 |
Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance at low temperatures. Moldable even in thin sections. Can be used in light-colored pro.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ISO 178 |
Chengdu Polyster H3303B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Excellent low-temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ boots, hose jack.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | |
Dow AFFINITY™ SM 8250 Polyolefin Plastomer AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ASTM D638 |
Arkema Group LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 8200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 82.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | Conditioned 15 days at 23°C - 50% RH; ISO178 |
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Asia Pacific) Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Flexural Modulus | 0.0400 GPa | 5.80 ksi | ASTM D638 |
Arkema Group LOTRYL® 17 BA 07 Copolymer Ethylene - Butyl Acrylate LOTRYL® 17 BA 07 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 07 is used as tie layer in coextrusion PP/PE, for extrusi.. |