Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl PPX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PPE-I-GF30
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Moisture Absorption 0.0400 %
0.0400 %
23°C / 50% RH
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
on Tensile Bar; SABIC Method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0070 cm/cm
0.0020 - 0.0070 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 3.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 75.0 MPa
10900 psi
ISO 2039-1
Tensile Strength at Break 80.0 MPa
11600 psi
5 mm/min; ISO 527
Elongation at Break 4.1 %
4.1 %
5 mm/min; ISO 527
Tensile Modulus 6.60 GPa
957 ksi
1 mm/min; ISO 527
Flexural Strength 120 MPa
17400 psi
2 mm/min; ISO 178
Flexural Modulus 5.50 GPa
798 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²
22.8 ft-lb/in²
80*10*4; ISO 180/1U
46.0 kJ/m²

@Temperature -30.0 °C
21.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 125 °C
257 °F
Rate B/50; ISO 306
128 °C
262 °F
Rate B/120; ISO 306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
IEC 60250
2.4

@Frequency 50.0 - 60.0 Hz
2.4

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm

@Thickness 3.20 mm
610 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.00030

@Frequency 50.0 - 60.0 Hz
0.00030

@Frequency 50.0 - 60.0 Hz
IEC 60250
0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 500 V
500 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2