Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ISO 527
Elongation at Yield 7.1 %
7.1 %
50 mm/min; ISO 527
Tensile Modulus 1.90 GPa
276 ksi
1 mm/min; ISO 527
Flexural Yield Strength 36.0 MPa
5220 psi
2 mm/min; ISO 178
Flexural Modulus 1.70 GPa
247 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af