Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 HI HV TS PA6 with impact modifier PA 6 higher viscosity, heat stabilized, impact modified for extrusion and blow molding. Automotive applications as air ducts and fuel filter pipes, fuel and oil containers.Information Provided by Pl.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100T BK602 is a toughened, high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where outstanding toughness is required.Informa.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 300TE BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 300TE BK602 is a medium-high viscosity toughened acetal homopolymer for injection molding with extremely low VOC emissions.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min |
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-1/-2 |
DSM Akulon® S223-TP4 Impact Modified Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
1mm/min; ISO 527-2/1A/1 |
SYNTHOS Forsan® 846 Acrylonitrile Butadiene Styrene (ABS) High impact, medium flow, glossy, suitableApplications: General purpose, transport packaging, furniture, leisure time equipmentContainers, suitcases, profiles, ABS sheets, skis, helmets, garden equi.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1mm/min; ISO 527 |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-1 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Total PS CPDS 849 High Flow, High Heat Resistance Polystyrene Total Petrochemicals Polystyrene 849 is a high flow, high heat resistant polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stabil.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Total PS CPDS 863 High Flow Flame Retardant Deca Polystyrene Total Petrochemicals Polystyrene 863 is a high flow, heat resistant, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensiona.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Eastman Provista ST Copolymer Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Tangent, MD; ASTM D882 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 EC PA12-CD25 Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process wit.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T BK602 is a toughened high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where o.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | >= 1.90 GPa @Temperature 100 °C |
>= 276 ksi @Temperature 212 °F |
Elasticity |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |