Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 60.0 kJ/m² | 9.52 - 28.6 ft-lb/in² | Average value: 41.5 kJ/m² Grade Count:19 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KE002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-kon* KE002 is a compound based on ACETAL COPOLY resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East) LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX92002 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KEL22A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL22A is a compound based on Acetal Homopolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RB003 PA 66 (Europe-Africa-Middle East) 15% glass beads filled polyamide 66 injection moulding resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WF0049XP PBT (Europe-Africa-Middle East) LNP* Thermocomp* WF0049XP is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NCFAG Copolymer 20% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 70.0 kJ/m² | 9.52 - 33.3 ft-lb/in² | Average value: 44.8 kJ/m² Grade Count:8 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 48.0 kJ/m² | 9.52 - 22.8 ft-lb/in² | Average value: 34.1 kJ/m² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |