Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 60.0 kJ/m² | 9.52 - 28.6 ft-lb/in² | Average value: 41.5 kJ/m² Grade Count:19 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 45.0 kJ/m² | 9.52 - 21.4 ft-lb/in² | Average value: 26.3 kJ/m² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180A |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 55.0 kJ/m² | 9.52 - 26.2 ft-lb/in² | Average value: 28.3 kJ/m² Grade Count:11 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V081 PPE+HIPS (Europe-Africa-Middle East) NORYL V081 is a high flow, UV stabilized PPO/PS blend for TV backplate applications. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features include Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MFM43S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFM43S is a compound based on Polypropylene resin containing Glass Fiber, Mineral. Added features include : Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RB008 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RB008 is a compound based on PA 66 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 70.0 kJ/m² | 9.52 - 33.3 ft-lb/in² | Average value: 44.8 kJ/m² Grade Count:8 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |