Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON PFD04ES PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON PFD04ES PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STATKON* PFD04ES is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 107 MPa
15500 psi
5 mm/min; ISO 527
Elongation at Break 2.6 %
2.6 %
5 mm/min; ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
1 mm/min; ISO 527
Flexural Yield Strength 152 MPa
22000 psi
2 mm/min; ISO 178
Flexural Modulus 5.90 GPa
856 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 112 µm/m-°C

@Temperature 23.0 - 60.0 °C
62.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 214 °C
417 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D257
Users viewing this material also viewed the following: