Dow Corning 24 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 24 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® 24 Emulsion is a stable, water-dilutable emulsion suitable for the food processing industry. It produces a slippery film upon water evaporation of the product.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.995 g/cc
0.995 g/cc
Volatiles 60 %
60 %
pH 6.5 - 8.5
6.5 - 8.5
Viscosity 100 cP
100 cP
dynamic
Descriptive Properties Value Comments
Appearance liquid