Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific)
PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ISO 294-4
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Linear Mold Shrinkage, Flow 0.0035 - 0.0060 cm/cm
0.0035 - 0.0060 in/in
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors..
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l..
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East)
LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS
LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR
Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Time 86400 sec
0.0030 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66
LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi..
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Time 86400 sec
0.0030 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6
LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 4.00 mm
0.0030 - 0.0060 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
LATI Latimass 37 B01-01 D025 Bio-Polymer
Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO 294-4
Celanese FORTRON 4332L6 PPS, Mineral / Glass Reinforced  (Unverified Data**)
Fortron 4332L6 is a glass fiber/mineral filled injection molding grade, which is intended for applications requiring improved tensile and flexural properties, when compared to other GF/MIN reinforce..