Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 107 MPa | 15500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Europe-Africa-Middle East) CYCOLOY MC5220 is a 20% glass reinforced PC+ABS blend for injection moulding purposes. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® 3412 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66 LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® PDR4908 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF14 L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF15 HS L BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF15 L BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mo.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PFD04ES PA 6 (Europe-Africa-Middle East) LNP* STATKON* PFD04ES is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill® PC GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D-882 |
Saint-Gobain Norton® High Performance Extruded PEI Film Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ISO value at 50 mm/min. |
BASF Capron® GR30 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ISO value at 50 mm/min. |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | ASTM D638 |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedChemically CoupledInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific) PPE+PS GF20% High Heat FR V-0 |
|||
Tensile Strength, Yield | 107 MPa | 15500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-30GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 107 MPa @Temperature -40.0 °C |
15500 psi @Temperature -40.0 °F |
ASTM D638 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |