SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing PTFE, Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 10.34 GPa
1500 ksi
50 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.87 J/cm
18.5 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 257 °C

@Thickness 3.20 mm
495 °F

@Thickness 0.126 in
unannealed; ASTM D648