Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne Nymax™ GF 1800 43 Black 22 Polyamide 612 (Nylon 612) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne Therma-Tech™ LC-5000C TC LCP
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Flexural Modulus | 10.27 GPa | 1490 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Solvay TECHNYL® SSD 330 KNF/E PA66, 15% glass filled, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, for injection molding specially stabilized to improves its resistance to automotive cooling liquids.Available in: Asia PacificProduct A.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.27 GPa | 1490 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RF0059 PA 66 (Asia Pacific) LNP STARFLAM* RF0059 is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X94104 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* 9X94104 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Chem Polymer Chemlon 215 GVH Nylon 6, 15% Glass Fiber Reinforced A glass fiber reinforced, flame retardant nylon 6. The material has a V0 flammability rating according to UL 94 testing procedure at thicknesses down to 1/16" (1.57mm).Data provided by the manufact.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.27 GPa | 1490 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst.. |