Material Notes:
Type AS-CEM Alumina-Silica Cement is a high temperature resistant cement useful for creating a hard coating on the surfaces of ZIRCAR® Alumina-Silica fibrous ceramic products or other porous insulating Materials. It has useful properties to 1260°C (2300°F). Information provided by Zircar Ceramics.
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 °C
3.00 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage 3.20 %

@Temperature 1260 °C,
Time 86400 sec
3.20 %

@Temperature 2300 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 37.2 %
37.2 %
Fe2O3 0.70 %
0.70 %
MgO 0.30 %
0.30 %
Na2O 0.70 %
0.70 %
Other 0.60 %
0.60 %
SiO2 59.1 %
59.1 %
TiO2 1.4 %
1.4 %
Electrical Properties Metric English Comments
Dielectric Strength 1.54 kV/mm
39.0 kV/in
Descriptive Properties Value Comments