Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1030HL Nylon 6/6  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1030HL Nylon 6/6  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: GM GMW3038P-PA66-GF30HForm: PelletsInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ASTM D570 and ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-2
186 MPa
27000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
2.0 %
2.0 %
ISO 527-2
Flexural Strength 262 MPa
38000 psi
ASTM D790
262 MPa
38000 psi
ISO 178
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
8.62 GPa
1250 ksi
ISO 178
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 9.03 kJ/m²
4.30 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
Unannealed; ISO 75-2/A
243 °C
470 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 20.5 kV/mm
520 kV/in
ASTM D149