AFE Technologies Cronite 657 Nickel Alloy Castings

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer AFE TEchnologies; North American Cronite
Trade Name Cronite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AFE Technologies Cronite 657 Nickel Alloy Castings.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AFE Technologies/North American Cronite, Inc.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 450 MPa
65300 psi
As Cast
Tensile Strength, Yield 230 MPa
33400 psi
As Cast
Elongation at Break 10 %
10 %
As Cast; 5.65 A<sup>0.5</sup>
Rupture Strength 8.80 MPa

@Temperature 1000 °C,
Time 3.60e+7 sec
1280 psi

@Temperature 1830 °F,
Time 10000 hour
Stress Rupture
15.0 MPa

@Temperature 950 °C,
Time 3.60e+7 sec
2180 psi

@Temperature 1740 °F,
Time 10000 hour
Stress Rupture
23.0 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
3340 psi

@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
34.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
4930 psi

@Temperature 1560 °F,
Time 10000 hour
Stress Rupture
48.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
6960 psi

@Temperature 1470 °F,
Time 10000 hour
Stress Rupture
64.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
9280 psi

@Temperature 1380 °F,
Time 10000 hour
Stress Rupture
100 MPa

@Temperature 700 °C,
Time 3.60e+7 sec
14500 psi

@Temperature 1290 °F,
Time 10000 hour
Stress Rupture