Axiall 50896 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 50896 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.33 g/cc
1.29 - 1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 54 - 60
54 - 60
delayed; ASTM D-2240
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 154 °C
310 °F