Mechanical Properties Metric English Comments
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 (Asia Pacific)
LNP* LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing PTFE, Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP KF006 Acetal Copoly
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled.
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0059 PA 66
LNP THERMOCOMP* RF0059 is a compound based on Nylon 66 resin containing 25% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RF0059 PA 66 (Asia Pacific)
LNP STARFLAM* RF0059 is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t..
Flexural Modulus 10.27 GPa
1490 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON LX04420C PEEK
LNP* STAT-KON* LX04420C is a compound based on Polyetheretherketone resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding Syst..