Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (Cond)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (Cond)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DAM; ASTM D792
Water Absorption 0.70 %
0.70 %
24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
0.125 in, DAM; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76
76
ASTM D785
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
73°F; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 282 - 299 °C
540 - 570 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.18 %
0.18 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 40 - 120 rpm
40 - 120 rpm