Polymer Property : Mold Temperature = 98.9 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 76.7 - 98.9 °C
170 - 210 °F
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Mold Temperature 76.7 - 98.9 °C
170 - 210 °F
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Mold Temperature 76.7 - 98.9 °C
170 - 210 °F
Polymer Resources PC-HH Polycarbonate, High Heat
Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource..
Mold Temperature 71.1 - 98.9 °C
160 - 210 °F
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Mold Temperature 76.7 - 98.9 °C
170 - 210 °F
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (DAM)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM)
Information provided by Ravago.
Mold Temperature 71.1 - 98.9 °C
160 - 210 °F
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (Cond)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company RTP 399 X 125087 A Polycarbonate (PC) Impact Modified - ESD Protection
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Average value: 82.2 °C Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company RTP 4300 B-322  Polysulfone/Polycarbonate Alloy (PSU/PC) Glass Fiber 22% - Flame Retardant
Glass Fiber 22% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company RTP 4300 B-360  Polysulfone/Polycarbonate Alloy (PSU/PC) Glass Fiber 30% - Flame Retardant
Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation.
Mold Temperature 79.4 - 98.9 °C
175 - 210 °F
RTP Company EMI 260.5 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company RTP 2000 B-322 Polysulfone Alloy, Glass Fiber
Mold Temperature 71.1 - 98.9 °C
160 - 210 °F
RTP Company EMI 863 Acetal (POM); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy
Data provided by Clariant Masterbatches
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company RTP 200E SI 2  Amorphous Nylon (Am. PA) Silicone 2%  (discontinued **)
Silicone 2%Comments:Silicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data ..
Mold Temperature 32.2 - 98.9 °C
90.0 - 210 °F
Average value: 55.4 °C Grade Count:23
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
RTP Company EMI 1761  Modified Polyphenylene Oxide (PPO) Shielding - Stainless Steel Fiber 10% &n
Shielding - Stainless Steel Fiber 10%Comments:EMI/RFI ShieldingESD ProtectionStainless Steel FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can ..