Ravago Manufacturing Americas Enviramid™ N1335HL BK Nylon 6/6

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N1335HL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedContains Recycled ContentRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 175 MPa
25400 psi
ASTM D790
Flexural Modulus 7.52 GPa
1090 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Unannealed; ASTM D648