Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 175 MPa | 25400 psi | |
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Flexural Strength | 175 MPa | 25400 psi | STN EN ISO 178 |
Plastcom SLOVASTER® B GF 20 FRK 3 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Flexural Strength | <= 175 MPa | <= 25400 psi | ISO 178 |
Polykemi AB POLYshine PBT D223 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | 175 MPa | 25400 psi | ASTM D790 |
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Flexural Strength | 175 MPa @Temperature 23.0 °C |
25400 psi @Temperature 73.4 °F |
ISO 178 |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Plastcom SLOVASTER® B1 GF 20 000/1 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticit.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
Nilit FRIANYL B63 TF-GV 1520 Nylon 6 for injection molding, 15% PTFE lubricated, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Strength | 175 MPa | 25400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Flexural Strength | 175 MPa | 25400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Flexural Strength | 175 MPa | 25400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Flexural Strength | 175 MPa | 25400 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DX02731C PC LNP STAT-KON* DX02731C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Flexural Strength | 175 MPa | 25400 psi | dry; ISO 178 |
DSM Novamid® 1010GN2-15Z BK701 PA6-GF15 FR(17) 15% Glass Reinforced, Flame Retardant, Easy Molding Grade, Injection Molding, High Flow |
|||
Flexural Strength | 175 MPa | 25400 psi | dry; ISO 178 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
Flexural Strength | 175 MPa | 25400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Strength | 175 MPa | 25400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide RF006K PA66, Glass Fiber Filled, Injection Molded Staramide RF006K is a Radiation Crosslinkable, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
Eurotec® Tecomid® NB40 GR15 NL PA 6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Ceradyne Ceralloy® BeO Applications:collector rodshelix supportswindowsFeatures: higher thermal conductivity at room temperature.Information provided by Ceradyne Company |
|||
Flexural Strength | 175 MPa | 25400 psi | Wet; ASTM D790 |
Asahi Kasei Leona® 14G25 25% Glass Filled Nylon 66 Enhanced strength and stiffness; with 25% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 615 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ASTM D790 |
Beijing Ranger Chem PBT-201-G25 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ASTM D790 |
Beijing Ranger Chem PBT-201-G25 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Strength | 175 MPa | 25400 psi | ISO 178 |
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Flexural Strength | 175 MPa | 25400 psi | |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |