Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® S RV250FR (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® S RV250FR (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
(Dry)
Water Absorption 2.5 %
2.5 %
initially dry
Moisture Absorption at Equilibrium 1.1 %
1.1 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
Elongation at Break 1.8 %
1.8 %
Tensile Modulus 11.0 GPa
1600 ksi
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
0.680 J/cm²

@Temperature 23.0 °C
3.24 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
50°C/h
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: