Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -20.0 °C |
17.6 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radiflam® S RV250FR (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV150 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -20.0 °C |
17.6 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop. Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |