Charpy Impact Unnotched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled
Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
DIN 53453
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled
Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® S RV250FR (cond.) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled
SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -20.0 °C
9.04 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -40.0 °C
9.04 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..