Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.680 J/cm²

@Temperature 23.0 °C
3.24 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® S RV250FR (cond.) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact, Notched 0.680 J/cm²

@Temperature 23.0 °C
3.24 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® CA HS (cond.) Nylon 66/6
Radilon® CA is a range of polyamide 66/6 copolymers obtained through the polymerization of hexamethylendiamine, adipic acid and caprolactam.Information provided by Radici group.
Charpy Impact, Notched 0.680 J/cm²

@Temperature -20.0 °C
3.24 ft-lb/in²

@Temperature -4.00 °F
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..