Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.050 %
0.050 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Hardness, Shore D 78
78
ASTM D2240
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Compressive Strength 68.9 MPa
10000 psi
10% Def.; ASTM D695
Compressive Modulus 1.10 GPa
160 ksi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256 Type A
Thermal Properties Metric English Comments
CTE, linear 119 µm/m-°C

@Temperature -40.0 - 149 °C
66.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM F433
Melting Point 171 °C
340 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 149 °C
300 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Constant 6.4

@Frequency 1e+6 Hz
6.4

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 10.2 kV/mm
260 kV/in
Short Term; ASTM D149
Dissipation Factor 0.165

@Frequency 1e+6 Hz
0.165

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Canada AG No
No
FDA Yes
Yes
NSF Yes
Yes
USDA Yes
Yes
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Color Natural
Machinability 3
1-10, 1=Easier to Machine