Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 171 °C | 340 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Melting Point | 171 °C | 340 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet) |
|||
Melting Point | 171 - 181 °C | 340 - 358 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |
|||
Melting Point | 171 - 181 °C | 339 - 357 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 171 °C | 340 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Melting Point | 171 °C | 340 °F | ASTM D3418 |
3M Dyneon™ PVDF 6020/1001 Polyvinylidene Fluoride
(discontinued **) Ultra-high molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabil.. |
|||
Melting Point | 171 - 190 °C | 340 - 374 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | DSC |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Melting Point | 171 °C | 340 °F | ASTM D3418 |
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Melting Point | 171 °C | 340 °F | ASTM D3418 |
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Melting Point | 171 °C | 339 °F | |
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r.. |
|||
Melting Point | 171 - 193 °C | 340 - 380 °F | |
Hexcel® HexWeb® TPU™ Thermoplastic Polyurethane Honeycomb Designation: Material-Cell Size (inches)-Film Gauge (inches)-Outer Skin Thickness.HexWeb® TPU™ is an attractive thermoplastic urethane honeycomb that has been developed using a proprietary fusing .. |
|||
Melting Point | <= 171 °C | <= 340 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Polybilt™ Bitumen Modifier 106 Low Density Polyethylene Resin Polybilt 106 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 106 content to achieve .. |
|||
Melting Point | 171 °C | 340 °F | ISO 3146 |
Eurostar Star L POM D74 POM, Injection Molded Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 171 °C | 340 °F | 10°C/min |
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melting Point | 171 °C | 340 °F | DIN 53765 |
BASF Ultraform® S1320 003 POM Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat.. |
|||
Melting Point | 171 °C | 340 °F | (Dry) |
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melting Point | 171 °C | 340 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Melting Point | 171 - 175 °C | 340 - 347 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 171 °C | 340 °F | 10°C/min |
Arkema Group Kynar® 6000 HDC N 119 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie.. |
|||
Melting Point | 171 °C | 340 °F | DIN 53765 |
BASF Ultraform S 1320 0021 UNC POM Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,.. |
|||
Melting Point | 171 °C | 340 °F | 10°C/min |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |
|||
Melting Point | 171 - 193 °C | 340 - 380 °F | ASTM D789 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |