Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 340 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 171 °C
340 °F
Crystalline, Peak; ASTM D3418
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Melting Point 171 °C
340 °F
Crystalline, Peak; ASTM D3418
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet)
Melting Point 171 - 181 °C
340 - 358 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Melting Point 171 - 175 °C
340 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Melting Point 171 °C
340 °F
Crystallinity by DSC; ASTM D 3418
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Melting Point 171 °C
340 °F
ASTM D3418
3M Dyneon™ PVDF 6020/1001 Polyvinylidene Fluoride  (discontinued **)
Ultra-high molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabil..
Melting Point 171 - 190 °C
340 - 374 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Melting Point 171 - 175 °C
340 - 347 °F
DSC
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition..
Melting Point 171 - 175 °C
340 - 347 °F
DSC
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Melting Point 171 °C
340 °F
ASTM D3418
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Melting Point 171 °C
340 °F
ASTM D3418
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Melting Point 171 - 193 °C
340 - 380 °F
Hexcel® HexWeb® TPU™ Thermoplastic Polyurethane Honeycomb
Designation: Material-Cell Size (inches)-Film Gauge (inches)-Outer Skin Thickness.HexWeb® TPU™ is an attractive thermoplastic urethane honeycomb that has been developed using a proprietary fusing ..
Melting Point <= 171 °C
<= 340 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Polybilt™ Bitumen Modifier 106 Low Density Polyethylene Resin
Polybilt 106 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 106 content to achieve ..
Melting Point 171 °C
340 °F
ISO 3146
Eurostar Star L POM D74 POM, Injection Molded
Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Melting Point 171 °C
340 °F
10°C/min
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Melting Point 171 °C
340 °F
DIN 53765
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
Melting Point 171 °C
340 °F
(Dry)
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Melting Point 171 °C
340 °F
10K/min; ISO 3146
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee..
Melting Point 171 - 175 °C
340 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Melting Point 171 °C
340 °F
10°C/min
Arkema Group Kynar® 6000 HDC N 119 PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie..
Melting Point 171 °C
340 °F
DIN 53765
BASF Ultraform S 1320 0021 UNC POM
Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,..
Melting Point 171 °C
340 °F
10°C/min
Arkema Group Kynar® 4000 HD PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b..
Melting Point 171 - 193 °C
340 - 380 °F
ASTM D789
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
Copyright © lookpolymers.com All Rights Reserved