Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | <= 1.00e+13 ohm | <= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 4240(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
Surface Resistivity per Square | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | ASTM D257 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Surface Resistivity per Square | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | ASTM D257 |
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | VDE 0303 |
GEHR Plastics POM-C Acetal Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | VDE 0303 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total PSI 4440(EU) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
DuPont Teijin Films Melinex® ST506 Polyester Film, 500 Gauge Melinex® ST506 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic.. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
DuPont Teijin Films Melinex® ST507 Polyester Film Melinex® ST507 is a slightly hazy, heat stabilized, polyester film. It has good handling characteristics and is recommended for silver circuitry applications, particularly where an adhesion topcoat.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 2901 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
CEN® Electronic Material BL Polyimide Film CEN®BL polyimide film is a printable film that has the same thermal and chemical properties as CEN®CN Polyimide Film, which offers excellent performance in temperatures from -269-400°C. CEN®BL i.. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer
(discontinued **) Description/Features:AntistaticInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |