Polymer Property : Thermal Conductivity = 0.216 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass
Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,..
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass
Data provided by the manufacturer, Owens Corning.
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet)
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet)
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM E1530
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet)
Thermal Conductivity 0.216 - 0.350 W/m-K
1.50 - 2.43 BTU-in/hr-ft²-°F
Average value: 0.294 W/m-K Grade Count:3
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Westlake Plastics Tempalux® 5000 Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi..
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM D2214
Ensinger TECAPEI® made from Ultem® 1000 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® H300 Acrylic
Superior UV protection, Adhesion to HIPS, ASTM Classification PMMA 0233V3Information provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® P-610 Acrylic
PVC Capstock, clear, low glossInformation provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® PB Acrylic
For PVC/acrylic alloys Information provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® A200 Acrylic
Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® P-600 Acrylic
PVC Capstock, clear, high glossInformation provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® P-601 Acrylic
PVC Capstock, white, high glossInformation provided by Arkema Group
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Arkema Group Solarkote® P-611 Acrylic
PVC capstock, white, low glossInformation provided by Arkema Group