Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering R80Z Natural Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering R80Z Natural Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural Rubber, 75-85 °IRHD. Formulated to meet BS1154 Grade Z80. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applications: Natural rubber offers low compression set, high tensile strength, high resilience and excellent resistance to tear and abrasion.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
-10% change after 168 hours @ 70°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 170 %
170 %
-15% change after 168 hours @ 70°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 40 %
40 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flash Point >= 300 °C
>= 572 °F
Copyright © lookpolymers.com All Rights Reserved