Victrex® PEEK 600P Polyetheretherketone  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® PEEK 600P Polyetheretherketone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliantInformation provided by Victrex
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
Melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
Result based on similar products; ISO 527
Elongation at Break 30 %
30 %
Result based on similar products; ISO 527
Tensile Modulus 3.70 GPa
537 ksi
Result based on similar products; ISO 527
Flexural Strength 150 MPa
21800 psi
Result based on similar products; ISO 178
Flexural Modulus 4.10 GPa
595 ksi
Result based on similar products; ISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
Result based on similar products; ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
Result based on similar products; ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: