Karina E 650D35/1-C Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 650D35/1-C Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.37 g/cc
1.32 - 1.37 g/cc
ASTM D 792
ASTM Color -2.02 - 0.98
-2.02 - 0.98
Color A, ME 12
1.82 - 4.82
1.82 - 4.82
Color B, ME 12
84.79 - 87.79
84.79 - 87.79
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 6.86 MPa
>= 996 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 36.0 kN/m
>= 205 pli
DIN 53507
Abrasion <= 340
<= 340
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application General Purpose Soles