Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F60R Fluorosilicone Rubber Red Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 60.Applications: S.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F80R Fluorosilicone Rubber Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications: |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F80X Fluorosilicone Rubber Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1,.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering J70M Butyl Rubber Bromobutyl Rubber, 65-75 IRHD. Brominated isobutylene-isoprene copolymer. To meet BS3227 Grade 70 and ASTM D2000 line call-out MBA708, F17.Applications: Bromobutyl is resistant to the same fluids a.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N40M Nitrile Rubber Nitrile Butadiene Rubber, 35-45 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Standard BS2751 BA40.Applications: Excellent resistance to petro.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N60C Nitrile Rubber Nitrile Butadiene Rubber (NBR). High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class "C", 55-65 IRHD. Approval ref.: 31/6.1... |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70C Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class D, approval ref.: 31/6.1... |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70V Nitrile Rubber Nitrile Butadiene/PVC Rubber, 65-75 °IRHD. Copolymer of acrylonitrile and butadiene blended with PVC.Applications: Excellent resistance in sealing applications against petroleum and mineral based f.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R70D Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 70 (NRQX70).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R70Z Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to meet BS1154 Grade Z70. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S50E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S50N Silicone Rubber Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. To meet UK Ministry of Defence Aircraft Materials .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S50Y Silicone Rubber Yellow Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. U.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60B Silicone Rubber Black Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60T Silicone Rubber Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United St.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65G Silicone Rubber Low Compression Set, Green Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65Z Silicone Rubber Low Compression Set, Grey Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compre.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S70H Silicone Rubber White Silicone Rubber, 68-78 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S80A Silicone Rubber Blue Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fe.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S80D Silicone Rubber Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Formulated to meet UK Ministry of Defence .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S80N Silicone Rubber Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z65L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 60-65 °IRHD. Low acrylonitrile content (ACN = 17%). ASTM designation = HNBR.Applications: High strength and excellent chemical resistance. Higher opera.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z85L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 81-90 °IRHD. Low acrylonitrile content.Applications: Specially compounded for service in low-temperature applications. High strength and excellent chem.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z90B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR. To meet ASTM D2000 line call-out M2DH920, A26, B16, EO16, EO36, F14.Ap.. |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |