Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants 541(NF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants 774VLF-WHITE (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants UniFlor 8512SB (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Resin Technology Group EN 239-2 Millennium™ UV Curable Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Cured |
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive UV MX 2230 is a one-component acrylate based polymer designed to be used as a quick-fixture, surface activated adhesive, (with optional UV or oven cure), for applications on a variety of substrates .. |
|||
Minimum Service Temperature, Air | <= -50.0 °C | <= -58.0 °F | |
Kazanorgsintez 158BK-20 Low Density Polyethylene Composite Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kaz.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
GEHR Plastics ABS Acrylonitrile Butadiene Styrene Acrylonitrile Butadiene Styrene copolymer has a good thermal and dimensional stability and scratch resistance. Advantagesgood mechanical strengthresists scratchinghigh surface strengthhigh impact st.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6166 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Low Temperature Flexibility |
Sylvin Technologies 6128-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Trelleborg R496 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Trelleborg R547 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 400601S SBS Based Material, 60A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
Adamas Adalon® 401 PTFE, 10% Polyimide Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
3M 8411 Edging and Reinforcing Tape 3M™ Edging and Reinforcing Tape 8411 is a transparent polyester film tape for many permanent edging and reinforcing types of applications.Information provided by 3M |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
3M 8412 Polyester Film Tape 3M™ Polyester Tape 8412 has excellent tensile strength and abrasion resistance, that can be used for many permanent edging and reinforcing types of applications.Information provided by 3M |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |