Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D 638 |
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound Information provided by PolyPlastic Group. |
|||
Tensile Strength, Yield | >= 10.0 MPa | >= 1450 psi | ASTM D412 |
Precision Polymer Engineering C70H Chloroprene Rubber Off-white, Chloroprene Rubber, 65-75 °IRHD. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regu.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering E63B Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Rubber, 55-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistance with .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ISO 527 |
Polimeri Europa Riblene® GM 20 Low Density Polyethylene - Coating Grade Riblene GM 20 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 20 is suitable for coating applications where a low neck-in is required. Moreover, for its rh.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering E80B Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistan.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering E80K Ethylene Propylene Rubber General purpose, peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet ASTM D2000/SAE J200 line call-out MCA810, A25, B35, F17... |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering N60R Nitrile Rubber Red Nitrile Butadiene / PVC elastomer blend 59-65°IRHD. Electrically non-conductive. Copolymer of acrylonitrile and butadiene, blended with polyvinyl chloride.Applications: Specially formulated as .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V75I Fluoroelastomer Compound Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1. Where Z1 = compressi.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V75Y Fluoroelastomer Compound Yellow Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = co.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V80G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = gre.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D412 |
Precision Polymer Engineering V80Q Fluoroelastomer Compound Black Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administr.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | Extension rate 2 in/min; ASTM D638 |
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkl.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
SABIC M200024 Linear Low Density Polyethylene for Injection Molding Product Description: M200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good f.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
SABIC M500026 Linear Low Density Polyethylene for Injection Molding Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Global D-2024 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 639 Perfluoroelastomer Chemraz® 639 perfluoroelastomer is specifically developed by Greene Tweed to meet the rigorous demands of aggressive plasma systems. This product’s unique formulation provides enhanced plas.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | heat aged 70 hours at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | 2"/min; ASTM D638 |
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | |
Trelleborg E647 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE7011 Profile Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent strength, good machinability, and foaming characteristics.Applications: Extrusion: profile extrusion.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Tensile Strength, Yield | 10.0 - 14.0 MPa | 1450 - 2030 psi | Average value: 11.2 MPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi.. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE1203 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Tensile Strength, Yield | 10.0 MPa | 1450 psi | ASTM D638 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |
|||
Tensile Strength, Yield | 10.0 - 85.3 MPa | 1450 - 12400 psi | Average value: 26.8 MPa Grade Count:173 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |