Material Notes:
Nitrile/PVC Rubber, 75-85 °IRHD. Copolymer of acrylonitrile and butadiene, blended with PVC. ASTM & ISO designation = NBR.Applications: Excellent resistance to petroleum based oils and fuels. Improved resistance to ozone and weather compared to standard nitrile grades.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
65 - 95
65 - 95
°IRHD, ±15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D412
7.00 - 13.0 MPa
1020 - 1890 psi
±30% change after 70 hours @ 100°C; ASTM D412
Elongation at Break 62.5 %
62.5 %
-50% change after 70 hours @ 100°C; ASTM D412
125 %
125 %
ASTM D412
Compression Set 50 %
50 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Non-brittle after 3 minutes
-30.0 °C
-22.0 °F
Flash Point >= 300 °C
>= 572 °F