Material Notes:
A high purity, ultrafine, wet ground, surface treated natural calcium carbonate available in dry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water based, solvent based, and high gloss powder coatings.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Brightness 95.5 %
95.5 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.050 %
0.050 %
Moisture Loss at 110°C % (dry)
Particle Size 0.70 µm
0.70 µm
Median Diameter
Specific Surface Area 9.5 m²/g
9.5 m²/g
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 5.5
Magnesium Carbonate % 1
Percent Finer than 1 Microns 65
Percent Finer than 2 Microns 90
Pounds Pigment/Solid Gallon (dry) 22.6
Retained in 325 mesh (dry) ppm 7
Treatment % 1.1