Polyram RamLloy PBB106 PC/ABS Alloy, UV Stabilized

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PBB106 PC/ABS Alloy, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV stabilized PC/ABS alloy for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 240 °C
17 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 4.50 J/cm
8.43 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
IEC 60250