Physical Properties Metric English Comments
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural
Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products..
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 265 °C
17 g/10 min

@Load 11.0 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East)
PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 260 °C
17 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific)
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East)
Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Melt Flow 17 - 22 g/10 min

@Load 2.16 kg,
Temperature 300 °C
17 - 22 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ISO 1133
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal  (Unverified Data**)
Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin
Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer.
Melt Flow 17 - 25 g/10 min
17 - 25 g/10 min
±15%
Kazanorgsintez 294-73 High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad..
Melt Flow 17 g/10 min

@Temperature 230 °C
17 g/10 min

@Temperature 446 °F
ASTM D1238
Kolon KOPEL® KP3372 General Purpose TPE Resin
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 260 °C
17 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133-1
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS.
Melt Flow 17 - 27 g/10 min
17 - 27 g/10 min
ASTM D1238
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly
EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer
Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai..
Melt Flow 17 - 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 - 23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman.
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene
DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor..
Melt Flow 17 - 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 - 23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman.
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 330 °C
17 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ISO 1133
Covestro Apec® 1745 Polycarbonate
Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (..
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
estimated from MVR using room temperature density; ISO 1133
Covestro Makrolon® 2556 Polycarbonate
MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Covestro Makrolon® OD2015 Polycarbonate
Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)  (Unverified Data**)
Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det..
Melt Flow 17 g/10 min

@Load 2.16 kg
17 g/10 min

@Load 4.76 lb
Dow HDPE 17450N High Density Polyethylene
DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability ove..
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17 g/10 min

@Load 4.76 lb,
Temperature 374 °F
(MVR) cm³/10min; ISO 1133
Celanese Hostaform® S 27242 XAP² ™ POM, Impact Modified  (Unverified Data**)
Easy flow, impact modified injection molding grade, with good low temperature impact strength and good weld line strength and reduced emissions. Emission according to VDA 275 < 5 mg/kgImpact modifie..
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved