Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 4010 MP PC/PBT-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND HI 40 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified blend PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents, good dimensional stabilit.. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer. |
|||
Vicat Softening Point | 120 °C @Load 1.00 kg, Thickness 4.00 mm |
248 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Micropol Isoplas P471 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Multibase Multi-Flamâ„¢ 205 HFRI Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Vicat Softening Point | 120 °C @Load 1.02 kg |
248 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis Bormed™ SC820CF Polypropylene Random Copolymer Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist.. |
|||
Vicat Softening Point | 120 °C @Load 5.00 kg |
248 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP 0540 GFC V0 Flame Retardant Polypropylene, 20% Glass Filled PP with 20% chemically coupled glass fiberFlame retardant class V0, excellent mechanical characteristics, excellent heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50N; ISO 306 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade Information provided by Eurotec® |
|||
Vicat Softening Point | 120 °C | 248 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CE 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |